HTR produces Natural Reclaim Rubber which is derived from old Used Scrap Natural Tube.

TECHNICAL DATA TEST METHOD STANDARD
·          Chemical Properties · ·
·          Acetone-Extract % ·          ASTM D 297-18 ·          7 – 15
·          Ash % ·          ASTM D 297-18 ·          13 – 27
·          Carbon Black % ·          ASTM E 1131 ·          13 – 27
·          RHC % ·          ASTM E 1131 ·          42 Min.
·          Physical Properties · ·
·          Specific Gravity (gm / cc) ·          ASTM D 297-93 ·          1.20 – 1.30
·          Tensile strength (Minimum) ·          ASTM D 412 ·          35 (Kg/Cm2) / 3.41 (Mpa)
·          Elongation ·          ASTM D 412 ·          225 Min.
·          Mooney Viscosity (1+4)@100’c) ·          ASTM D 1646 ·          20 – 50
·          Hardness at Shore “A” ·          ASTM D 2240 ·          55 – 65