HTR produces Butyl Reclaim Rubber GRADE HTR 1001 from old used scrape of Butyl Tube with well equipped production machinery & Modern Laboratory.

TECHNICAL DATA   TEST METHOD STANDARD
·          Chemical Properties · ·
·          Acetone-Extract % ·          ASTM D 297-18 ·          6 – 12
·          Ash % ·          ASTM D 297-18 ·          2 – 6
·          Carbon Black % ·          ASTM E 1311 ·          28 – 36
·          RHC % ·          ASTM E 1131 ·          50 Min.
·          Physical Properties · ·
·          Specific Gravity (gm / cc) ·          ASTM D 297-93 ·          1.10 – 1.14
·          Tensile strength (Minimum) ·          ASTM D 412 ·          75 (Kg/Cm2) / 7.35 (Mpa)
·          Elongation ·          ASTM D 412 ·          480 Min.
·          Mooney Viscosity (1+4)@100’c) ·          ASTM D 1646 ·          35 – 55
·          Hardness at Shore “A” ·          ASTM D 2240 ·          50 – 60
Benefits ::
Rapid and Efficient Mixing Decreased Power Usage.
Minimal Heat Accumulation during Processing.
Stable Thermo Plasticity.
Accelerated Curing Rates.
Superb Long-Term Durability.
Cost-Efficiency
:: Facts ::
Incorporating reclaimed rubber in production saves about 70% energy compared to virgin rubber.
India leads globally in reclaim rubber production.
It ranks fifth worldwide in synthetic rubber consumption.